All Products

 

 

 
 
 

Product

 
 
 

Description

 
 
 

Reference

 
 
 
 
 
 
 
 
 
 
 
 
 

Nanodiamond powder of laser synthesis,

possibility of customized surface functionalization.

 
 
Average grain size: 4.0-5.0 nm, ash residue: ˂0.02 wt.%
 
 
 
 
 
 
 
 
 
 

Nanodiamond powder of laser synthesis, hydroxylated & nitrogenized;

metal free;

for biomed research

 
 
Average grain size: 4.0-5.0 nm, Hydrophilic, PL, Lyophobic, ash residue: ˂0.02 wt.%
 
 
 
 
 
 
 
 
 
 

Nanodiamond powder of laser synthesis, modified, metal free, ferro-magnetic (un-known nature);

for scientific research

 
 
Average grain size: 4.0-5.0 nm, luminescent, Magnetic, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 
 
 

Detonation nanodiamond powder, specially purified, graphite & metal free, non-functionalized

 
 
Average grain size: 3.0-6.0 nm, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 
 
 

Detonation nanodiamond powder, purified, modified, alkylated;

for ceramics, for some of polymer resines, for nuclear research.

 
 
Average grain size: 3.0-6.0 nm, Hydrophobic, Lyophobic, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 
 
 

Detonation nanodiamond powder, purified, hydroxylated;

for electroplating & polishing, coolants, water soluble polymers

 
 
Average grain size: 3.0-6.0 nm, Hydrophobic, Lyophobic, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 
 
 

Detonation nanodiamond powder, purified, Fe-doped,

for optic coatings & magnetic nano-fluids, bio-research

 
 
Average grain size: 3.0-6.0 nm, Ferro-magnetic, high photoluminiscence, ash residue: ˂0.8 wt.%
 
 
 
 
 
 
 
 
 
 

Detonation nanodiamond powder, purified, modified, alkylated & nitrogenized;

for aceton colloids & aceton soluble rubbers

 
 
Average grain size: 3.0-6.0 nm, Hydrophobic, Lyophobic, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 
 
 

Crushed High Pressure High Temperature nanodiamond powder, purified, modified, hydroxylated;

for polishing slurries

 
 
Average grain size: 30-50 nm, Hydrophilic, Lyophobic, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 

High Pressure High Temperature Crushed nanodiamond powder, purified, modified, hydroxylated & nitrogenized, for plating

 
 
Average grain size: 30-50 nm, Hydrophilic, Lyophobic, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 
 
 

1.7 wt. % disaggregated nanodiamond water suspension (RayND),

pH: 3.5-4.5;

for R&D, bio applications

[The price is planned to drop]

 
 
Average grain size: 4.0-5.0 nm, Stable.
 
 
 
 
 
 
 
 

4 wt.% nanodiamond water suspension;

Nitrogenized RayND, highly dispersed;

for biomedical research

[The price is planned to drop]

 
 
Average grain size: 4.0-5.0 nm, high photoluminiscence, Stable.
 
 
 
 
 
 
 
 
 
 

1.7 wt. % nanodiamond water suspension(disaggregated RT-DND),

pH=3.5-5.5;

forpolishing, inks, water soluble polymers

 
 
Average grain size: 3.0-6.0 nm, disaggregated single particles, Stable.
 
 
 
 
 
 
 
 
 
 

4 wt. % nanodiamond water suspension (RT-DND), highly dispersed, pH of wide range;

for water soluble polymers, inks, sensors

 
 
Average grain size: 3.0-6.0 nm, Stable.
 
 
 
 
 
 
 
 
 
 

4 wt. % nanodiamond acetone suspension,

highly dispersed,

for HIPS and ABS rubbers and other acetone soluble polymers

 
 
Average grain size: 3.0-6.0 nm, Stable.
 
 
 
 
 
 
 
 
 
 

5 wt. % nanodiamond isopropyl alcohol suspension (RayND),

highly dispersed,

for seeding in CVD diamond growth

 
 
Average grain size: 4.0-5.0 nm, Stable.
 
 
 
 
 
 
 
 
 
 

5 wt. % nanodiamond N-methyl-2-pyrrolido-ne suspension, highly dispersed;

for textiles, resins, plastics, inks, sensors

 
 
Average grain size: 3.0-6.0 nm, High luminescence, Stable.
 
 
 
 
 
 
 
 
 
 

10 wt. % nanodiamond 2-Butoxyethanol suspension,

highly dispersed;

for varnishes, herbicides, latex paints, enamels

 
 
Average grain size: 3.0-6.0 nm, Stable.
 
 
 
 
 
 
 
 
 
 

7 wt. % nanodiamond xylene suspension, highly dispersed;

for varnishes, paints, polishes, wafers and PCB cleaning agents

 
 
Average grain size: 3.0-6.0 nm, Stable.
 
 
 
 
 
 
 
 

5 wt.% nanodiamond slurry,

for lapping, inner surfaces flow polishing, electroplating, contains hydroxylated crashed HPHT-ND

requires sonication before handling

 
 
Average grain size: 40-50 nm
 
 
 
 
 
 
 
 

3 wt.% HPHT nanodiamond slurry,

highly dispersed in deionized water,

for finishing

 
 
Average grain size: 40-50 nm, high photoluminiscence, Stable.
 
 
 
 
 
 
 
 
 
 

7 wt. % nanodiamond cyclohexane suspension,

highly dispersed,

additive to anionic elastomers

 
 
Average grain size: 3.0-6.0 nm, Stable.
 
 
 
 
 
 
 
 
 
 

10 wt. % nanodiamond water-based gel;

pH of wide range;

for lapping, finishing, running-in, polishing, cooling, ultrasonic cleaning

pretreatment at CVD & PVD

 
 
Average grain size: 3.0-6.0 nm, Stable.
 
 
 
 
 
 
 
 
 
 

3 wt. % nanodiamond polyester oil colloid,

highly dispersed,

additive to lubricants, lapping / finishing / running-in

 
 
Average grain size: 3.0-6.0 nm, Stable.
 
 
 
 
 
 
 
 
 
 

Nanodiamond additive to antifriction synthetic oils;

recommended dilution for finishing 1/25, for running-in 1/50

 
 
Average grain size: 3.0-6.0 nm, Stable., based on BVA-68
 
 
 
 
 
 
 
 
 
 

10 wt. % nanodiamond organic-based grease for fine polishing of diamonds, CVD diamond films, optic crystals & ceramics

 
 
Average grain size: 3.0-6.0 nm, Stable.
 
 
 
 
 
 
 
 
 
 

5 wt. % nanodiamond antiwear grease for lapping,

finishing, running-in of gears, engines, generators and precision parts

 
 
Average grain size: 3.0-6.0 nm, Stable., Washed off with water
 
 
 
 
 
 
 
 
 
 

Detonation nanodiamond powder, purified, modified, hydroxylated & nitrogenized;

for high quality slurries & coolants

 
 
Average grain size: 3.0-6.0 nm, high photoluminiscence, Hydrophilic, Lyophobic, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 
 
 

Detonation nanodiamond powder, purified, modified, alkylated & siliconized;

for polymer compounds

 
 
Average grain size: 3.0-6.0 nm, Hydrophobic, Lyophobic, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 
 
 

Carbon nanotubes hydroxylated, soluble in water;

for composite materials

 
 
75 wt.% single wall CNT, Hydrophilic, Lyophobic
 
 
 
 
 
 
 
 
 
 

10 wt. % nanodiamond dimethylformamide suspension,

highly dispersed,

for acrylic fibers, plastics, synthetic leathers, glues

 
 
Average grain size: 3.0-6.0 nm, Stable.
 
 
 
 
 
 
 
 

20 wt.% nanodiamond water slurry,

additive to electrolytes in galvanic coatings for improving wear & corrosion resistance

 
 
Stable., Recommended dilution 1/40, or 0.5 -0.6 wt. % ratio in electrolyte
 
 
 
 
 
 
 
 

20 wt.% nanodiamond water slurry,

additive to electrolytes in Ni Electroless coatings for wear & corrosion resistance

 
 
Stable., Recommended dilution 1/40, or 0.5 -0.6 wt. % ratio in electrolyte