Carbon Nano - Powders

 

 

 
 
 

Product

 
 
 

Description

 
 
 

Reference

 
 
 
 
 
 
 
 
 
 
 
 
 

Nanodiamond powder of laser synthesis,

customized surface functionalization.

The price is planned to drop.

 
 
Average grain size: 4.0-5.0 nm, ash residue: ˂0.02 wt.%
 
 
 
 
 
 
 
 
 
 

Nanodiamond powder of laser synthesis, hydroxylated & nitrogenized;

metal free;

for biomed research

 
 
Average grain size: 4.0-5.0 nm, Hydrophilic, PL, Lyophobic, ash residue: ˂0.02 wt.%
 
 
 
 
 
 
 
 
 
 

Nanodiamond powder of laser synthesis, modified, metal free, ferro-magnetic (un-known nature);

for scientific research

 
 
Average grain size: 4.0-5.0 nm, PL, Magnetic, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 
 
 

Nanodiamond powder of detonation synthesis, specially purified, graphite & metal free, non-modified;

for various applic.

 
 
Average grain size: 3.0-6.0 nm, ash residue: ˂0.1 wt.%, Polydispersed
 
 
 
 
 
 
 
 
 
 

Detonation nanodiamond powder, purified, modified, aminated;

for compatible polymer compound

 
 
Average grain size: 3.0-6.0 nm, Hydrophobic, Lyophobic, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 
 
 

Detonation nanodiamond powder, purified, eliminated radicals;

for metal & ceramic composites, dry lubrication, nuclear appl.

 
 
Average grain size: 3.0-6.0 nm, Hydrophobic, Lyophobic, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 
 
 

Detonation nanodiamond powder, purified, hydroxylated;

for electroplating & polishing, coolants, compatible polymers (PE)

 
 
Average grain size: 3.0-6.0 nm, Hydrophobic, Lyophobic, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 
 
 

Detonation nanodiamond powder, purified, nitrogenized;

for syn. oils, IPA, NMP, Cy, DMSO & acetone colloids & soluble rubbers

 
 
Average grain size: 3.0-6.0 nm, high photoluminiscence, Hydrophobic, Lyophobic, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 
 
 

Detonation nanodiamond powder, purified, ethylated;

for compatible polymers, paints, lacquers, inks, synth. oils, polishes, slurries

 
 
Average grain size: 3.0-6.0 nm, Hydrophobic, Lyophobic, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 
 
 

Detonation nanodiamond powder, purified, Fe-doped,

for optic coatings & magnetic nanofluids, bio-research

 
 
Average grain size: 3.0-6.0 nm, Ferro-magnetic, high photoluminiscence, ash residue: ˂0.8 wt.%
 
 
 
 
 
 
 
 
 
 

Detonation nanodiamond powder, purified, nitrogenized;

for stable solvent-based polymer additives, H₂O, DMSO, Cy, IPA, NMP

 
 
Average grain size: 3.0-6.0 nm, high photoluminiscence, Hydrophilic, Lyophobic, ash residue: ˂0.1 wt.%
 
 
 
 
 
 
 
 
 
 

Detonation nanodiamond powder, purified, alkylated & aminated;

for sintering and compatible polymers (PA)

 
 
Average grain size: 3.0-6.0 nm, ash residue: ˂0.1 wt.%, Highly hydrophobic & lyophobic
 
 
 
 
 